Hi, I'm 100% newbie, and I have some polished aluminum rims on my car, and I want to chrome plate them. I need help on what to buy, and how to do it myself, is this possible? please help me.....
|
|
||||
|
I answered this in the other forum before seeing it here.
Even half a rim would need a couple of hundred amps of power and a very large amount (30 Gallons or so) of solution to plate. Are you willing to invest several thousand dollars to get set-up to do this? There's also a learning curve to plating; you're not going to be able to just set-up the kit, dump your rims in and out they come plated. If you're serious about learning to chrome plate, and have never plated before, we suggest starting by buying a 2 Gallon nickel plating kit, read the manual, become an expert at nickel plating. Then, invest in a Triple Chrome kit....but even then, it's just not practical to think you'll be able to plate bumpers and rims. Better to leave bumpers and rims to the plating shops and concentrate on the smaller items.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Plating Guitar Tremolo w/ Smoked Chrome (newbie) | taorama | Plating Pot Metal | 1 | 09-07-2005 08:12 AM |
| Plating Problem grey finish from chrome plating | tshirah | Electroplating Questions | 2 | 08-13-2005 12:08 AM |
| Newbie question about copper plating cabinet hinges | superdav | Electroplating Questions | 7 | 07-13-2005 12:31 AM |
| chrome plating plastic dash QUESTION | gtolovedaddy | Electroplating Questions | 0 | 08-25-2004 06:11 PM |
| Chrome (re)plating question - howto | olaf_sc | Electroplating Questions | 1 | 07-29-2003 02:00 PM |