Default "Sandwiching" Acid Copper

Gents,

I am using high-build acid copper over a flash copper strike. After I am done sanding down the acid copper, do I need to apply another layer of flash copper over the sanded-down acid copper layer (sandwich the acid copper between flash copper layers) or do I simply continue with the rest of the layers on top ?

Copy Chrome is going to follow on top.

Thanks,

Ares
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 08-27-2004, 09:19 PM
Moderator
 
Join Date: Feb 2003
Location: southeast
Posts: 199
bhhodges is on a distinguished road
Default

no you dont need to add another layer of flash copper.

bill
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Acid copper Gabourie Electroplating Questions 3 09-25-2004 09:42 PM
filling small pits with acid copper danderson Electroplating Questions 2 08-25-2004 08:55 AM
Acid copper plating problem! Attention Fibergeek Gabourie Electroplating Questions 10 08-15-2004 12:24 AM
where do i get battery acid for my copper kit plater12 Electroplating Questions 1 07-17-2004 09:49 PM
Strike Copper or Acid Copper over Nickel? mdarr Electroplating Questions 2 07-13-2003 02:53 AM


All times are GMT -4. The time now is 04:52 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.