Default hard chrome plating

what all mat\'ls. can be hard chrome plated. i know steel, cast iron and aluminum, what about brass and bronze? are there others? thanks for your help and the forum is really nice. dave
Reply With Quote
  #2 (permalink)  
Old 12-26-2001, 11:43 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,361
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: hard chrome plating

Most materials can be hard chromed, including brass and bronze.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
hard chrome plating dcarter Electroplating Questions 4 04-27-2008 10:21 PM
Hard Chrome Plating Help dg5240 Electroplating Questions 0 05-31-2005 03:17 PM
Need help hard chrome plating an internal diameter... ld2222 Electroplating Questions 6 12-31-2004 05:15 PM
Plating Hyd. Valve Spools w/ Hard Chrome Daveleeander Electroplating Questions 0 04-27-2004 02:55 PM


All times are GMT -4. The time now is 12:36 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.