Default alum. turned a smutty gray (Electroless Chrome)

I fellowed the instructions to the letter. from sp degreasing,break water
test, zinkiating, rainse, and dip in hot chrome solution for 60 min!!
And it turned out a smutty gray, and will not buff out to a shine
My part looked better before the chrome

Solution was just off of a boil
zin. solution was 76*
Sp degreaser was 185*
Distilled Water was used in everything

ANY HELP THAT ANYBODY COULD GIVE WOULD BE GREAT

DOGWOODDIR
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Electroless Krome VS Copy Chrome plating? qwik3r Electroplating Questions 3 04-29-2004 12:39 AM
Price of Copy Chrome vs. electroless Krome plating dwthomas Electroplating Questions 1 05-14-2003 11:01 AM
tripple chrome, nickel chrome, copy chrome or electroless ch magfinpete Electroplating Questions 1 05-19-2002 01:52 PM
Electroless Nickel over Chrome gglines Electroplating Questions 1 05-13-2002 12:09 AM
Electroless Chrome Surface Prep. wilfbryan Electroplating Questions 1 05-03-2002 08:58 PM


All times are GMT -4. The time now is 09:31 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.