i was wondering if the copper/chrome combo kit is a good way to start chroming car parts. is it ok to not have a nickel plating step in the process? will the chrome not stick as well to copper? also, what are the differences (besides procedure and equipment) to the electroless and anode type systems? what are the pros and cons of each?
thanks, justin |
|
||||
|
The chrome will adhere fine to the copper plate, but the chrome gets a lot of its color from the underlying nickel plate. If you want an authentic chrome plate, it\'s best to use the nickel.
Besides the procedure and equipment, there are no differences between electroless and anode systems. The end result is exactly the same.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 10:11 AM |
| Nickel bath inexplicably quits plating | jackf | Electroplating Questions | 5 | 01-25-2005 10:55 PM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 03:52 AM |
| Electroless Krome plating Q's | chcarver | Electroplating Questions | 1 | 10-10-2002 11:00 PM |
| Plating process. | Dean | Electroplating Questions | 1 | 01-02-2002 01:18 AM |