I have just started plating as a hobby and I have ran into my first snag. While plating aluminium with electroless krome, bubbles appear to be underneath the plating. I degreased the aluminium with acetone then zincated it first. What am I doing wrong
|
|
||||
|
This problem is addressed in the manual and can be solved by aerating the part with larger bubbles from an airstone during plating.
Please use our technical support section at http://www.caswellplating.com/support.htm to post further technical support related issues. This forum is not set up to handle requests properly and in a timely fashion.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Problems with LCD, looking for suggestions! | Sid03 | Anodizing Questions | 5 | 01-16-2004 04:52 AM |
| Consistency Problems | NeoMoses | Anodizing Questions | 6 | 12-13-2003 03:01 PM |
| Problems with LT1 Intake Manifold | thesound | Metal Polishing Questions | 4 | 11-16-2003 08:54 PM |
| What is the right amount of bubbles to see with Copy Cad? | emobley | Electroplating Questions | 9 | 06-27-2003 02:40 AM |
| Copper over nickel problems | mixter1313 | Electroplating Questions | 1 | 05-23-2002 05:19 PM |