Default Plastic Chrome Plating

Hi, I am interested in your plating kits. But I have some quections with them. First I will spray the parts with Conductive Paint, then plated with copper. Afterwards, can I use Copy Chrome Kits to get the same quality of Commercial Chorme-Plated Products? Or the triple chrome kit is more suitable?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 08-03-2002, 04:06 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: Plastic Chrome Plating

If you want a commercial quality chrome plate, the only option is the Triple Chrome kit. It\'s the only kit we sell that gives a REAL chrome plate and uses standard commercial techniques to get the required finish.

The Triple Chrome kit includes copper, nickel and chrome plating kits.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #3 (permalink)  
Old 08-04-2002, 01:46 AM
Newbie
 
Join Date: Jul 2002
Posts: 26
mr.wagon
Default Re: Re: Plastic Chrome Plating

Thank you, but how long time need plating the object for each plating process?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #4 (permalink)  
Old 08-04-2002, 10:07 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: Plastic Chrome Plating

Copper - approx 15 mins.
Nickel - approx 10 mins.
Chrome - approx 2 mins.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #5 (permalink)  
Old 08-04-2002, 11:50 PM
Newbie
 
Join Date: Jul 2002
Posts: 26
mr.wagon
Default Re: Re: Plastic Chrome Plating

Quote:
caswell wrote:
Copper - approx 15 mins.
Nickel - approx 10 mins.
Chrome - approx 2 mins.
How about the Voltage and Amp ?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #6 (permalink)  
Old 08-05-2002, 12:43 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: Plastic Chrome Plating

Copper - 1-6V, 0.05-0.1 amps/sq in
Nickel - 1-6V, 0.05-0.06 amps/sq in
Chrome - 3-12V, 1.0-1.5 amps/sq in
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #7 (permalink)  
Old 08-05-2002, 02:54 AM
Newbie
 
Join Date: Jul 2002
Posts: 26
mr.wagon
Default Re: Plastic Chrome Plating

Thank you, and are the heaters in Triple Chrome Kit (2Gal) operate at 110v? And how many Watt do they consume? And do you have any transformer change 220v to 100/110v since electricity voltage of Hong Kong is 220v?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #8 (permalink)  
Old 08-05-2002, 10:49 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: Plastic Chrome Plating

They\'re 300Watt heaters. You can source them locally at an aquarium dealer.

We don\'t sell converters.

We also won\'t be able to send you the Triple Chrome kit to Hong Kong. It\'s classified as Dangerous Goods for transportation. We can ship this product to California, then you could arrange your own shipping to Hong Kong.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #9 (permalink)  
Old 08-05-2002, 11:11 AM
Newbie
 
Join Date: Jul 2002
Posts: 26
mr.wagon
Default Re: Re: Plastic Chrome Plating

If then I will take the Copy Chrome Kit instead of it. How about the Watt consume of the heaters in Copy Chrome Kit and Copper Plating Kit?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #10 (permalink)  
Old 08-06-2002, 09:35 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: Plastic Chrome Plating

They\'re the same.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 08:35 AM
chrome plating plastic dash QUESTION gtolovedaddy Electroplating Questions 0 08-25-2004 07:11 PM
Chrome plating plastic services needed. qwik3r Services Offered/Wanted 0 02-08-2004 04:45 PM
chrome plating on plastic jean Services Offered/Wanted 1 04-20-2003 09:28 PM
Remove chrome plating from plastic vdubcoop Electroplating Questions 3 08-20-2002 11:12 AM


All times are GMT -4. The time now is 05:26 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.