I should have wrote "achieving a chrome-like finish" on large objects, mostly non-metallic.
I put off buying the Silvachrome a while back and now see that it's discontinued and that my best bet is Silvaspray and a plating kit. My question is, how do I do something as large as a car bumper. A tank is needed right? Someone directed me to Mirrachrome by Alsa Corp. it's a one-part chemical that can be clearcoated. But, it's expensive! Does Caswell make anything similar to Silvachrome in terms of ease of application? Thanks, Owen |
|
||||
|
By ease of application, do you mean difficult? Silvachrome, and similar processes by other companies, are not as easy as they may appear. The biggest problem with these products is yellowing of the topcoat. We discontinued the product because people had so much difficulty getting good results.
Plating real chrome onto your nonmetallic bumper will be just as difficult and impractical. Send it to a plater.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| need advice about chroming kits | darrell | Electroplating Questions | 3 | 08-24-2005 04:57 PM |
| Hard chroming? | motorbuilder | Electroplating Questions | 9 | 07-23-2005 03:35 PM |
| large part finish? | slamed150 | Metal Polishing Questions | 4 | 07-11-2004 10:03 PM |
| Chroming anodized aluminum. | hifi | Electroplating Questions | 4 | 08-05-2003 12:23 PM |
| Plating really small objects | edsel | Electroplating Questions | 1 | 06-13-2002 07:10 PM |