I used a plating process in the past that was called \"Selectron Brush Plating\", and from looking at the plating kits, it seems to be that the process is quite similar (it would have to be). I have some ideas for use of the nickel and chrome plating process that would have fit well with the \"Selectron Brush Plating\" process, but I guess they are no longer in the business. Ergo, I come to you, to see if it would be practical to attempt using your processes, to plate the surface area of 20 to 40 square inches, to a depth of less than 1,000th of an inch.
__________________
Dean Thames |
|
||||
|
Sure.
What metal are you plating and what is the base metal? Are you committed to brush plating, or would immersion plating be ok too?
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 09:11 AM |
| Plating Problem grey finish from chrome plating | tshirah | Electroplating Questions | 2 | 08-13-2005 12:08 AM |
| Nickel bath inexplicably quits plating | jackf | Electroplating Questions | 5 | 01-25-2005 09:55 PM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 02:52 AM |
| Electroless Krome plating Q's | chcarver | Electroplating Questions | 1 | 10-10-2002 10:00 PM |