Old 08-06-2002, 05:36 PM
Newbie
 
Join Date: Aug 2002
Posts: 7
felix
Default what is the difference between .....

Electroless nickel and \"regular\" nickel other than method of how the plating is applied?
Reply With Quote
  #2 (permalink)  
Old 08-06-2002, 07:02 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: what is the difference between .....

The method of application is the only difference.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 08-22-2002, 09:41 AM
Amateur Metal Finisher
 
Join Date: May 2002
Posts: 84
48Buick
Default Re: what is the difference between .....

There are a couple differences along with how its applied.
Electroless is usually thinner plating then the electrolytic type.
Also instead of anodes to give up metal for plating the metal comes out of the solution and onto the part.
Eventually the solution will have to be replentished.

48 Buick
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
What is the difference between Chrome and Nickel? remotestartdepot Electroplating Questions 1 01-08-2005 07:03 PM
what is the difference between............... duke Electroplating Questions 1 08-09-2003 10:49 AM
Difference in Buffing machines... dwoodru1 Metal Polishing Questions 3 05-29-2003 04:26 AM
Whats the difference between the buffing and grinding units? july_favre Metal Polishing Questions 3 12-27-2002 01:15 AM
whats the difference? gopedhead Electroplating Questions 5 04-07-2002 12:27 PM


All times are GMT -4. The time now is 06:05 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.