I've been experimenting trying to plate with nickel. The anode has a smokey haze that will come off with steelwool if I rub hard enough. It seems like some of the parent material is also coming off in layers and the under layer is like new. Is there a pickle or something that I can put it in to do a better job?
|
|
||||
|
Don't waste your time. Just wire wool it.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| How to plate Nickel over old Nickel when steel shows through | ASHENASH | Electroplating Questions | 3 | 04-22-2005 03:03 AM |
| Dealing with partially nickel plated steel | AresP | Electroplating Questions | 3 | 08-19-2004 10:41 PM |
| Nickel problems | Eddy | Electroplating Questions | 0 | 04-23-2004 11:31 AM |
| Chrome, Nickel or copy chrome? | dwthomas | Electroplating Questions | 1 | 02-15-2003 01:49 PM |
| Replating Nickel | shorton | Electroplating Questions | 7 | 11-06-2002 11:36 AM |