Is it possible to put nickel or copper plating over auto body repair liquid steel. I've got a part that I can't put welding heat on it. So i'm tring to get some alternative.
Tkx for the help! |
|
||||
|
These epoxies are plastics filled with very finely ground steel. Unfortunately, the epoxy encapsulates the steel particles and insulates them from each other, and the art being repaired.
So, it doesn't work, sorry.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
||||
|
However, PITSTOP is an epoxy filled with silver. It's expensive, but it works. Fill the deep holes with steel epoxy, then wipe a thin layer of Pitstop over it to provide conductivity.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Plating Nitrocarburized mild steel | MrRage | Electroplating Questions | 0 | 08-19-2005 02:26 PM |
| Filling pits in steel in preparation for nickel plating | pastorclyde | Electroplating Questions | 2 | 07-13-2005 10:50 AM |
| Plating aluminum on steel | TheMartin | Electroplating Questions | 0 | 04-23-2004 08:26 PM |
| Copper plating on stainless steel 316L strip/sheet | slee36 | Services Offered/Wanted | 0 | 03-31-2004 01:46 PM |
| Plating Advice for 12L14 Steel ?? | kenitd | Electroplating Questions | 1 | 01-27-2003 08:03 PM |