Thread: Remove chrome plating from plastic

  1. #1

    Default Remove chrome plating from plastic

    How can I remove chrome plating from automotive plastic parts??
    Will Muratic acid or acetic acid eat away the plastic I need something safe to use on the underlying part.

    Thanks for the help.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #2
    Join Date
    Nov 2001
    Location
    Lyons, NY USA
    Posts
    1,794

    Default Re: Remove chrome plating from plastic

    You can very carefully reverse plate the chrome off, using an acid pickle. You should be able to remove the chrome layer down to the nickel underneath without harming the plastic.

    It\'s unlikely that a bit of acid on the plastic will harm it anyway....after all the acid probably came in a plastic container, right?

    You can also buff it off.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com
    Have A Web Site?
    Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. #3

    Default Re: Remove chrome plating from plastic

    Where can one purchase or make this \"acid pickle\"??
    When the chrome is removed what can be done to remove the nickel that is left on? Buff it off from there maybe?
    thanks
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  4. #4
    Join Date
    Nov 2001
    Location
    Lyons, NY USA
    Posts
    1,794

    Default Re: Remove chrome plating from plastic

    There\'s a formula in our plating manual. http://www.caswellplating.com/complete.htm It\'s mostly battery acid.

    If you want to remove the nickel also, there is another pickle you can use, or you can buff it off.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com
    Have A Web Site?
    Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. copy chrome vs triple chrome plating
    By splbnd27 in forum Electroplating Questions
    Replies: 18
    Last Post: 06-21-2006, 07:35 AM
  2. chrome plating plastic dash QUESTION
    By gtolovedaddy in forum Electroplating Questions
    Replies: 0
    Last Post: 08-25-2004, 06:11 PM
  3. Chrome plating plastic services needed.
    By qwik3r in forum Services Offered/Wanted
    Replies: 0
    Last Post: 02-08-2004, 03:45 PM
  4. chrome plating on plastic
    By jean in forum Services Offered/Wanted
    Replies: 1
    Last Post: 04-20-2003, 08:28 PM
  5. Plastic Chrome Plating
    By mr.wagon in forum Electroplating Questions
    Replies: 9
    Last Post: 08-06-2002, 08:35 AM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1