My company has been thinking about setting up to do the Copy Chrome process by the first of the year. The biggest piece we would probably ever do would be like this Valve Cover on my Straight 8
![]() its about 12\" X 30\" total plus maybe 16\"sq for the ends Would a 16 Gal Copper \"for fill and repair\" and 16 Gal Copy Chrome kit with the 60 amp Rectifier work for something this size? If so would I need Custom Tanks for valve covers? Thanks for any info Jdee |
|
||||
|
Yes, all that would work.
You could plate half of the item, then turn it around and plate the other half, or you could build a custom tank and transfer the solution. We don\'t list a 16 Gal Copy Chrome Kit, but give us a call and we\'ll put a quote together for you.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| using aluminum as a cathode | scocklin | Anodizing Questions | 19 | 03-31-2007 12:18 AM |
| Need opinions on my next tank. | jtsuttle | Anodizing Questions | 4 | 03-29-2004 12:32 PM |
| tank size vs acid concentration | whistule | Anodizing Questions | 28 | 11-16-2003 04:34 PM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 02:52 AM |
| tank size & rectifier | neil | Electroplating Questions | 3 | 04-04-2002 11:44 PM |