Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Electroplating Questions

Notices

Electroplating Questions Discussion Board For Electroplating and Electroless plating.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 02-24-2005, 11:59 AM
Newbie
 
Join Date: Dec 2004
Posts: 2
DennyDwyer
Default plug + plate

I have a set of golf irons that are chrome plated and show considerable wear. Will the plug +plate system do the job on this?
Reply With Quote
  #2 (permalink)  
Old 02-27-2005, 12:34 PM
Moderator
 
Join Date: Feb 2003
Location: Texas
Posts: 269
dadkar2 is on a distinguished road
Default

I'm not convinced plug n plate is for large parts. I use it extensively for small parts; eg, screws, small finials, finishing nails, etc--especially with gold. I much prefer immersion plating. Gold is tough to do as an immersion plating process due to the cost and shelf life issues. So I always plug n plate with gold.

Also, the nickel levelers and brighteners don't really have a chance to do their job with the plug n plate method.

Ken
Reply With Quote
  #3 (permalink)  
Old 02-27-2005, 12:35 PM
Moderator
 
Join Date: Feb 2003
Location: Texas
Posts: 269
dadkar2 is on a distinguished road
Default

Oh, one more thing. For touch up repair, plug n plate is great too.

Ken
Reply With Quote
  #4 (permalink)  
Old 03-01-2005, 12:37 AM
Amateur Metal Finisher
 
Join Date: Jul 2002
Location: Florida
Posts: 69
gsw3 is on a distinguished road
Default Shelf life of gold?

Ken, how long is the shelf life of the gold solution for tank plating?

I just ordered/recieved a quart (2) weeks ago along with a 24ct. gold anode.

I have read some posts about the gold settling out of the solution (after some period of time) and then it is shot.

Just wondering.


BTW: The gold plating I am doing is coming out fantastic.
I saved the company over $800.00 during the first 2 minutes of gold plating thanks to Caswell's supplies.



Side question:
Could I use a 14ct anode (verses the 24ct anode)?
Reason: To have a more durable (harder) gold surface for electrical contacts (I have a few old 14ct rings I could melt down to make anodes).
Will any adverse effects (such as screwing up the solution) crop up?

Thanks!

George W.
Orlando, FL
Reply With Quote
  #5 (permalink)  
Old 03-01-2005, 06:57 AM
Moderator
 
Join Date: Feb 2003
Location: Texas
Posts: 269
dadkar2 is on a distinguished road
Default

George,

I really can't give you an infornmed answer on either question. These are best left to Caswell's support. I understand some had a concern about the shelf life and Caswell were investigating it with the supplier, but I never heard the resolution of that. It has been a few weeks.

As far as the anode, I don't believe the gold solution dissolves the anode in any case, so the gold will come out of the solution--not out of the anode material. In this case, Caswell's stainless steel anode is all you need. You might check with him and then update us in this posting.

Ken
Reply With Quote
  #6 (permalink)  
Old 03-01-2005, 06:58 AM
Moderator
 
Join Date: Feb 2003
Location: Texas
Posts: 269
dadkar2 is on a distinguished road
Default

Oh, one more thing. I have had my latest batch of FastGold for over 2 years and it is still in solution, just fine.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Plug n Plate Gold over Sterling novenarosary Electroplating Questions 0 03-12-2004 10:00 PM
Plug n Plate lphurley Electroplating Questions 3 09-23-2003 12:15 AM
Plug N Plate Question carmelmike Electroplating Questions 1 03-20-2003 06:10 PM
Plug & Plate a Beltline?? ecoglio Electroplating Questions 1 03-05-2003 06:51 PM
Plug N Plate Copy Chrome question Great_Scott Electroplating Questions 5 03-20-2002 05:53 PM


All times are GMT -4. The time now is 06:07 PM.