Ok Guy\'s, I\'m almost there. One more question. I have the triple chrom plating kit. In the manual it says the mist suppressior, sulfuric acid, and catalyst are already in the catalyst. My question is do I need to add sulfuric acid as the instructions on the bag says, or is it already in the mixture. Thanks for a great site.................Buddy
|
|
||||
|
All you have to add is:
1. chrome powder 2. catalyst 3. distilled water The sulfuric acid is now pre-mixed with the chrome solution.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Copy chrome and resistance to rust, tarnish, dulling? | phunkmastakrez | Copy Chrome Kit Customers Only | 6 | 08-25-2005 10:13 AM |
| Copy Chrome Start-up | Elitefisherman | Electroplating Questions | 10 | 04-18-2004 05:24 AM |
| Chrome plating solution | blackleg | Electroplating Questions | 3 | 02-19-2004 07:33 PM |
| Chrome (re)plating question - howto | olaf_sc | Electroplating Questions | 1 | 07-29-2003 03:00 PM |
| Hard chrome vs triple chrome | butters | Electroplating Questions | 1 | 02-20-2003 12:35 AM |