I have several antique gold-plated jewelry items that have suffered more than one alteration over the generations, leaving patches of soft solder residue on the backs. I suspect that much of it is lead solder.
I intend to purchase a Plug'n'Plate System, Fastgold and thickening powder to disguise this unappealing situation. To prepare the surface for the gold, do I need a nickel kit, a copper kit, or the combination kit; and use them in what order, over the lead solder? And over the non-lead solder? I see that Flash Copper isn't available in PnP formula; is an undercoat of PnP nickel a valid substitute? Must I use Pickle, or would that loosen the delicate soldered-on attachments? It's a lot to absorb; thank you for your help, Evangeline. |
|
||||
|
PNP Copper IS Flash Copper. Make sure the lead is very clean, then it should plate fine.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Can I Copy Chrome over Solder? Possible Tumbler issue? | waylonh | Electroplating Questions | 4 | 08-20-2005 02:51 PM |
| 24k vs 18k FastGold | jump | Electroplating Questions | 2 | 04-22-2005 09:44 PM |
| Stripping solder / gold plating pcb fingers | clab | Other Metal Finishing Questions | 0 | 07-27-2004 05:32 PM |
| anodizing solder aluminum | buckeyevs | Anodizing Questions | 3 | 02-27-2004 06:20 PM |
| Aluminum Solder Paste | trw | Other Metal Finishing Questions | 2 | 03-25-2003 09:55 AM |