I would like to plate approximately 0.000200 nickel and then 0.000030 gold on copper PCB edge connector pins. I only have about 100 connectors to do for a hobby project so time is not a problem. Can I use the plug and plate system and get the plating thicknesses that I want and the durability that I would need or would I be better off with one of the other kits?
|
|
||||
|
Yes, Plug N Plate will work fine. Just keep testing your thickness and apply more if required.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
||||
|
Not really - if you don\'t already have the equipment to do that, it\'s quite expensive.
I assumed from your precise thickness requirements that you had a way to measure this already. You can use a masking liquid to mask off whichever sections you don\'t want tin plated. See http://www.caswellplating.com/maskit.htm
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 09:11 AM |
| Going For The Gold | gsw3 | Electroplating Questions | 3 | 09-11-2005 12:18 PM |
| How about Gold on Gold ? | Ra | Electroplating Questions | 5 | 10-12-2004 07:47 PM |
| gold PCB edge contact plating | fargap | Electroplating Questions | 2 | 07-27-2004 07:24 PM |
| Silver polish on 24k gold plate?? | chromo | Electroplating Questions | 3 | 04-07-2003 05:14 AM |