Is anyone familiar with this plating process? I am looking to plate some brass connectors with this plating and would like to know A) if an underplate is needed, and how thick it should be. Can it be plated direct?
Application is for coaxial connectors. Thanks. |
|
|||
|
we are doing this plating on connectors since 12 years
our E-MAIL sunmetal61@yahoo.co.in for further qur. Regards Yogesh |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| PLATING POT METAL............... | 48Buick | Plating Pot Metal | 31 | 08-29-2007 12:40 PM |
| Plating over cold metal casting | jh2ohouse | Electroplating Questions | 2 | 12-16-2006 09:28 PM |
| Plating pot metal for corrosion protection before painting | rspencer | Plating Pot Metal | 2 | 08-03-2004 12:39 AM |
| Refinishing Metal Golf Club Heads | BillSchultz | Other Metal Finishing Questions | 0 | 08-17-2003 11:40 AM |
| Pot Metal Plating questions | Dave | Electroplating Questions | 1 | 04-03-2002 06:37 PM |