Hey folks,
I just received my complete wheel kit $4000 http://www.caswellplating.com/kits/wheelchrome.html , and started my chroming process. All goes well up intil the copy chrome part... I am doing aluminium. The zincate goes well, the copper flash goes well, but now the ?'s :- ) 1. I received the copy crystals in a 5 gallon bucket not in premeasured bags. I also received plastic bottles of nickle brightner. DO I put the distilled water plus the copy crystals PLUS the nickle brightner? I do have them in the amounts they stated on the site in my bath (1.5 gallons distilled water, 35 oz copy crystals, and 4 oz Nickle brightner) 2. What tempreture should I keep the copy chrome mixture at during the plating process? Thanks guys! |
|
|||
|
Well first off, all the question you are asking should be in the manual. The copy chrome and nickle use the same instructions. That being said, yes mix all three together heated to 110 deg F and stir it until the crystals are dissolved. Then let it sit for 24 hours before using it. Heat to 110 deg F for plating.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| triple chrome vs. nickel/chrome vs. copy chrome | spectraflamed | Electroplating Questions | 4 | 01-21-2007 10:07 AM |
| copy chrome vs triple chrome plating | splbnd27 | Electroplating Questions | 18 | 06-21-2006 07:35 AM |
| Copy Chrome Start-up | Elitefisherman | Electroplating Questions | 10 | 04-18-2004 04:24 AM |
| Copy Chrome Questions | junodale | Electroplating Questions | 13 | 03-17-2004 11:15 AM |