I am new to plating and have a couple of questions before I jump in.
- I need to chrome plate some small parts ( < 1 sq inch serface area ). I am wanting to nickle plate first to build up the surface about .005 and smooth out any scratches. Then chrome plate. The objects are steel. Can this be done with the plug-n'-plate product? I would like to dip plate to have a more even coverage. If dip plating in using plug-n'-plate do you have to use an anode. And if so what kind? Thanks jed |
|
|||
|
nickle will not fill scratches, you will have to polish them out of the steel before plating or build with copper and polish out. You cannot plug-n-plate chrome at all. If you want a chrome look, use copy chrome and as with nickle you will have to get the scratches out first. More than likely, you can use the brush as an anode for dipping.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 10:11 AM |
| Nickel bath inexplicably quits plating | jackf | Electroplating Questions | 5 | 01-25-2005 10:55 PM |
| First time plating, some questions.... | vic valis | Electroplating Questions | 1 | 09-29-2003 06:39 PM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 03:52 AM |
| Electroless Krome plating Q's | chcarver | Electroplating Questions | 1 | 10-10-2002 11:00 PM |