Question SECONDARY BRIGHTENER for nickel

I want formula of SECONDARY BRIGHTENER for bright nickel bath
Reply With Quote
  #2 (permalink)  
Old 09-02-2005, 02:17 PM
jimcarry's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: SECONDARY BRIGHTENER for nickel

All chemical make ups are on your MSDS these sheets I believe should be sent when ever you purchase a product from Caswell’s even Hobby platers should have a complete list of MSDS on every thing they use this is for there safety and knowledge. All MSDS can be sent to you via e-mail or snail mail from Caswell’s
__________________
Jim Eaton
Reply With Quote
  #3 (permalink)  
Old 09-03-2005, 02:14 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: SECONDARY BRIGHTENER for nickel

MSDS are sent on request, and only show materials that may pose a hazard. All our chemical formulae are proprietary.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 09:01 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.