Default tank heater rubber ends deteriorating

Just set up he chrome tank, (triple chrome plate system) and plated a dummy and a piece of copper tube, I then started to clean up, pulled the anodes out and the heater, Well, the heater rubber ends are deteriorating fast.
I had black rubber all over my gloves, this better not be contaminating my Chrome tank. Answers please
Also the rubber suction cup swelled so bad that it fell off the heater.

Last edited by TOMB; 10-02-2005 at 07:38 PM.
Reply With Quote
  #2 (permalink)  
Old 10-03-2005, 07:45 AM
jimcarry's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: tank heater rubber ends deteriorating

Quote:
Originally Posted by TOMB
Just set up he chrome tank, (triple chrome plate system) and plated a dummy and a piece of copper tube, I then started to clean up, pulled the anodes out and the heater, Well, the heater rubber ends are deteriorating fast.
I had black rubber all over my gloves, this better not be contaminating my Chrome tank. Answers please
Also the rubber suction cup swelled so bad that it fell off the heater.
My heaters did the same thing and i had no problem with contamination
__________________
Jim Eaton
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 02:49 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.