I have been unable to find any information on your site with regard to what must be done with any of the chemicals once they have been used. Do instructions come with each chemical or is it assumed that all the chemicals must be handled by qualified waste disposal people?
Many thanks - Stuart |
|
||||
|
There are detailed disposal techniques explained in our plating manual.
You can take steps to reduce the quantity and toxicity of chemicals before they are disposed of properly, usually at a municipal dump HAZMAT station.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Waste | modifyit15 | Electroplating Questions | 2 | 02-01-2004 01:25 AM |
| LT sealer disposal | desert_roamer | Anodizing Questions | 0 | 12-27-2003 01:45 PM |
| Chemical Disposal | ZackRobertson | Electroplating Questions | 1 | 02-12-2003 10:08 AM |