Default Gold solution seperated....

I hadn't used my gold plating solution for about a year and when I went to use it the gold had deposited on the sides of the bottle. I have only poured solution out of this bottle and haven't poured any used solution back in, so I don't understand why this happened. Shaking the bottle has no effect. Is there something I can do to get the gold to redissolve in the solution? Thanks for your help.

Regards, Larry
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
gold plating solution gone bad?????? anyone from there ?? clocktools Electroplating Questions 2 08-21-2008 06:44 PM
trouble plating with 18K fast gold solution didierphmartin Electroplating Questions 2 05-06-2008 02:51 PM
Temperature of Caswell gold solution apricotscrub Electroplating Questions 0 03-13-2004 06:36 PM
I know your gold plating solution is cyanide free, but... tbloss001 Electroplating Questions 1 07-30-2003 02:23 PM
14k gold solution Rusty Armstrong Electroplating Questions 1 04-05-2002 10:23 PM


All times are GMT -4. The time now is 09:24 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.