-- Lance Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm Please support the moderators on our site by leaving reputation for their helpful posts. Read more here. |
|
|||
|
Thank you. It is not clear that it is a product. When tied to the other recipes. I think as a marketing stand point you need to point this out other than.........
PICKLE #4 is a free flowing mixture of dry acids. instead..... PICKLE #4 is a free flowing mixture of dry acids developed by Caswell and offered as a product. My 2 cents |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Mixing the pickle Baths | Tim1hd | Electroplating Questions | 4 | 05-10-2005 05:02 PM |
| Aluminium trim adonizing removal? | SP4SPD | Metal Polishing Questions | 7 | 07-27-2004 12:14 AM |
| pickle #4 | fxstcguy98 | Electroplating Questions | 0 | 02-15-2004 11:01 PM |
| Pickle #4? | mdarr | Electroplating Questions | 1 | 07-24-2003 02:17 PM |
| Can you electro strip chrome with pickle #3? | tbloss001 | Electroplating Questions | 3 | 06-06-2003 09:36 AM |