I am a fishing lure manufacturer.
One of the things I make is lead spoons.
I would like to have them nickel or chrome plated.
I would like to do this myself, but I don't think I have time to experiment or to learn. Would someone be interested in plating these?
Would this be difficult to learn or have done?
Also would like to plate some fishing lures.

Thanks,
David
Reply With Quote
  #2 (permalink)  
Old 02-08-2006, 08:07 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: plating lead

I will be glad to help in any way I can, if you would like I could plate them or I can try to walk you through the steps...
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Improving Plating Performance jimcarry Electroplating Questions 0 09-28-2005 08:50 AM
Gold Plating and Nickel plating tzmandevil Electroplating Questions 2 09-16-2005 09:11 AM
plating over lead and/or aluminum-based filler m1garandusa Electroplating Questions 1 10-21-2003 11:18 PM
Plating Stainedglass wraped in Lead midnightblue Electroplating Questions 1 03-02-2003 09:18 AM
plating and size power? chromo Electroplating Questions 7 01-18-2003 02:52 AM


All times are GMT -4. The time now is 03:36 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.