Default Chrome or Powder - SCAM?

I came across this on another forum i belong to what do you guys think about this?
http://cgi.ebay.com/ebaymotors/Yamaha-Suzuki-Harley-Kawasaki-Ducati-COLOR-CHROME-RIMS_W0QQitemZ4617048706QQcategoryZ34284QQssPageNa meZWDVWQQrdZ1QQcmdZViewItem
__________________
Jeff B.
Instructions for riding a Warrior: 1) sit on bike, 2) start bike and idle till warm, 3) pull in clutch and put in gear, 4) release clutch and rip on the throttle, 5) {VERY IMPORTANT!!} HOLD THE F*** ON!!!, 6) Enjoy!! Side effects may include whiplash, wrinkle free skin, and an evil smile resembling the "Joker".
Reply With Quote
  #2 (permalink)  
Old 03-02-2006, 07:27 PM
lcaswell's Avatar
Caswell Inc President
 
Join Date: Jan 2001
Location: Lyons NY USA
Posts: 2,326
Blog Entries: 3
lcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud of
Default Re: Chrome or Powder - SCAM?

It's a liquid spray on system, with a color added into the topcoat...similar to the Silvachrome system we used to sell.

We stopped selling it because the topcoat would yellow after a time.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote
  #3 (permalink)  
Old 03-03-2006, 05:54 PM
BigDog's Avatar
Amateur Metal Finisher
 
Join Date: Dec 2004
Posts: 89
BigDog is on a distinguished road
Default Re: Chrome or Powder - SCAM?

Quote:
Originally Posted by lcaswell
It's a liquid spray on system, with a color added into the topcoat...similar to the Silvachrome system we used to sell.

We stopped selling it because the topcoat would yellow after a time.
Thank you for clearing this up for me. I was feeling a scam but hey you never know....
__________________
Jeff B.
Instructions for riding a Warrior: 1) sit on bike, 2) start bike and idle till warm, 3) pull in clutch and put in gear, 4) release clutch and rip on the throttle, 5) {VERY IMPORTANT!!} HOLD THE F*** ON!!!, 6) Enjoy!! Side effects may include whiplash, wrinkle free skin, and an evil smile resembling the "Joker".
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Fs: Turnkey Powder Coating And Ceramic Coating Business!!!! Mcurtis7 Used Items For Sale 0 10-02-2005 02:18 PM
Lolly Pop Powder on a Chrome Surface.. Powder is cracking!! tattoome5150 Powder Coating Questions 5 06-18-2005 11:46 PM
Can I chrome over powder coating? kv1370 Powder Coating Questions 8 12-05-2004 11:29 AM
Powder Coating (Chrome) Question... TCalYen Powder Coating Questions 3 05-12-2004 11:24 AM
Opinions on chrome powder bgillis17 Powder Coating Questions 1 09-23-2003 03:38 PM


All times are GMT -4. The time now is 06:26 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.