Default % Sulfuric in Battery Acid?

I bought battery acid at an auto parts store to anodise with and the salesman said is was 100% sulfuric acid. It worked well at 50%. I bought some more later that was MUCH cheaper for a larger quantity at another store that didn't work so hot at 50%. Is it possible that it was diluted? Does anyone know what the dilution rate is for battery acid? Is there a better source for sulfuric?
Reply With Quote
  #2 (permalink)  
Old 12-05-2002, 08:02 PM
Newbie
 
Join Date: Dec 2002
Posts: 6
jime
Default Should have...

...read other posts on the subject before, as it seems they answered most of my questions! Looks like i should use straight 'battery acid' and not dilute it. Is there a way to test the ratio in the solution?
Reply With Quote
  #3 (permalink)  
Old 12-05-2002, 09:44 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

You can test the specific gravity of the solution with a Hydrometer.

http://www.freasglass.com/battery.htm
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #4 (permalink)  
Old 01-26-2003, 07:35 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Buy Battery Acid from NAPA Auto Stores, product # 9002. It is a consistantly high quality product.
Specific gravity = 1.26
Pure sulfuric acid (reagent grade) is 98%
Battery acid is 1 part reagent grade to 2 parts distilled water.

Our instructions call for BATTERY ACID, which then has to be diluted.

The reason for this is that reagent grade is very difficult for the amateur plater to find, whereas battery acid is easy.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Acid SniperSlayer Anodizing Questions 8 07-25-2005 09:59 PM
Where to buy sulfuric acid? jlister Anodizing Questions 2 11-14-2004 09:56 PM
where do i get battery acid for my copper kit plater12 Electroplating Questions 1 07-17-2004 08:49 PM
Acid for anodizing desert_roamer Anodizing Questions 5 07-25-2002 09:10 PM
Battery Acid. ketanjajal Electroplating Questions 1 03-05-2002 09:27 AM


All times are GMT -4. The time now is 05:19 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.