2 years ago I purchased the electroless nickle kit and used it very succesfully. Today I topped up the mix and put in the parts that I spent 2 days sanding and polishing. I hour later they came out, crappy looking. Some areas are unplated, some have a dull grey area. I am guessing the bath has gone bad from sitting. No problem, I will mix up a fresh batch. Question is, do I need to go back to the buffing wheel and make them beautiful again before I replate them? What a pain.
Second question. Is there something besides string that I can use to hang the parts from? String is a pain.What about stainless steel wire? Thanks in advance. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Nickle "Plug-N-Plate" question HELP!! | pyro1711 | Electroplating Questions | 1 | 08-03-2004 10:29 PM |
| "high phosphorus" electroless nickel? | jkellymcc | Electroplating Questions | 0 | 08-26-2003 06:35 PM |
| Black Krome over Electroless Krome? | athomas | Electroplating Questions | 2 | 08-26-2003 02:49 PM |
| electroless nickel vs regular nickel | Rocky | Electroplating Questions | 1 | 07-24-2003 03:12 PM |
| tank for electroless nickel | jpb531 | Electroplating Questions | 1 | 04-03-2002 06:18 PM |