Hi! I have a silver plated Conn 20K Sousaphone. I would like to have the inside of the bell copper plated. What would be the best kit to use for this? I was thinking that a plug & plate kit would be too small since the bell is 26" in diameter. Also, is there anybody out that could possibly do this for me if I decide that its too much for me to do?
|
|
||||
|
The Plug N Plate Copper Kit should work well for this. It may take you a while to plate, and I'd get an extra bottle of solution, but it should be easy to do and give good results.
An immersion kit would be tricky to use for this application.
__________________
-- Lance Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm Please support the moderators on our site by leaving reputation for their helpful posts. Read more here. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Keep getting blisters in flash copper plating...HELP | gtabadboy | Electroplating Questions | 7 | 11-17-2005 08:19 PM |
| Improving Plating Performance | jimcarry | Electroplating Questions | 0 | 09-28-2005 08:50 AM |
| I did a dumb thing - now how do I remove copper plating? | Mark3316 | Other Metal Finishing Questions | 0 | 05-19-2005 02:57 PM |
| Differet copper plating questions, plus copy chrome/ nickel? | krsimulis | Electroplating Questions | 1 | 07-26-2004 12:25 AM |
| Copper plating on stainless steel 316L strip/sheet | slee36 | Services Offered/Wanted | 0 | 03-31-2004 12:46 PM |