Default Zinc Plating the Inside of an Ashtray

Having problems getting the inside of an auto ashtray plated with zinc, using Copy Cad. The size of the ashtray is roughly 1" wide, 3" long and 2" deep. What can I do to get the plating inside the ashtray?

donald
Reply With Quote
  #2 (permalink)  
Old 06-13-2006, 11:24 AM
Amateur Metal Finisher
 
Join Date: Dec 2003
Posts: 203
fxstcguy98 is on a distinguished road
Default Re: Zinc Plating the Inside of an Ashtray

You will have to make an anode that will fit down inside the ashtray that is about 1/2" away from all the sides and bottom. Wire the auxiliary anode to the other anodes in the tank and it should throw alot better.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Zinc Plating an old auto radio case engineerscott Electroplating Questions 1 02-18-2006 01:08 AM
Improving Plating Performance jimcarry Electroplating Questions 0 09-28-2005 08:50 AM
Zinc plating on running seal surface? Broke Electroplating Questions 1 12-06-2004 01:52 PM
CopyCad & Zinc failure - electrolyte problems? seanc Electroplating Questions 4 11-08-2004 09:16 AM
Plating Tank - Zinc aermakov@rogers.com Electroplating Questions 1 03-27-2003 01:38 PM


All times are GMT -4. The time now is 03:04 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.