Sorry, we don't have any information on this, mainly because the bluing that occurs on chrome is somewhat of a mystery itself. It usually only occurs on low quality chrome jobs.
If you want to experiment, get a Copy Chrome Plug N Plate Kit, plate a small steel item and heat it up to see if it blue's.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Copy Chrome | warchild | Electroplating Questions | 1 | 03-18-2005 03:43 PM |
| Copy Chrome Start-up | Elitefisherman | Electroplating Questions | 10 | 04-18-2004 04:24 AM |
| Detail chrome plating for show parts!! | GOD12A | Electroplating Questions | 0 | 01-11-2004 11:08 PM |
| Plating and high heat | chromo | Electroplating Questions | 1 | 01-29-2003 01:15 AM |
| Heat effects on Chrome | nunnc | Electroplating Questions | 1 | 06-16-2002 10:55 PM |