Yes, it makes it harder.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
||||
|
No, it holds its shine much longer.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| triple chrome vs. nickel/chrome vs. copy chrome | spectraflamed | Electroplating Questions | 4 | 01-21-2007 11:07 AM |
| copy chrome vs triple chrome plating | splbnd27 | Electroplating Questions | 18 | 06-21-2006 08:35 AM |
| Copy chrome and resistance to rust, tarnish, dulling? | phunkmastakrez | Copy Chrome Kit Customers Only | 6 | 08-25-2005 10:13 AM |
| Tarnish or Corrosion of Copy Chrome | Westy | Electroplating Questions | 2 | 08-23-2005 10:43 AM |
| Copy Chrome Start-up | Elitefisherman | Electroplating Questions | 10 | 04-18-2004 05:24 AM |