2-4 volts and 0.003 - 0.007 amps per square inch (when tank plating)
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
||||
|
Sort of....the volts are the same, but the amps don't apply. You want to start at 2 volts and increase until it starts plating.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 09:11 AM |
| How about Gold on Gold ? | Ra | Electroplating Questions | 5 | 10-12-2004 07:47 PM |
| Power Supply Requirements | KomaToast | Electroplating Questions | 1 | 02-26-2004 11:19 PM |
| Silver polish on 24k gold plate?? | chromo | Electroplating Questions | 3 | 04-07-2003 05:14 AM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 02:52 AM |