Default copy chrome

Do you think copy chrome will work well on aluminum and magnesium?I want to plate alot of parts from my and my wifes bikes.I also like the idea of no toxic chemicals.
Could I also start with a small kit then eventually move upto aluminum bike wheels with bigger tanks and more chemicals?Thank you, Shawn
Reply With Quote
  #2 (permalink)  
Old 07-03-2006, 07:56 AM
jimcarry's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: copy chrome

Shawn
yes this will work on the metals you are talking about I would recommend starting out with a small kit and working your way up
__________________
Jim Eaton
Reply With Quote
  #3 (permalink)  
Old 07-03-2006, 02:19 PM
shawnkloker's Avatar
Newbie
 
Join Date: Jun 2006
Posts: 20
shawnkloker is on a distinguished road
Default Re: copy chrome

Thanks,Jim.My only concern now is that I want to see more pics of parts plared with copy chrome. Shawn
Reply With Quote
  #4 (permalink)  
Old 07-03-2006, 03:06 PM
jimcarry's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: copy chrome

Here are some pictures of a pot metal part plated with copy chrome system or you can go to my picture gallery http://forum.caswellplating.com/phot...0/ppuser/17870 copy chrome is the only plating kit i use
Attached Thumbnails
copy-chrome-radio-face.jpg  
__________________
Jim Eaton

Last edited by jimcarry; 07-03-2006 at 03:08 PM.
Reply With Quote
  #5 (permalink)  
Old 07-03-2006, 06:13 PM
shawnkloker's Avatar
Newbie
 
Join Date: Jun 2006
Posts: 20
shawnkloker is on a distinguished road
Default Re: copy chrome

Jim,Looks real good.Thanks, Shawn
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
triple chrome vs. nickel/chrome vs. copy chrome spectraflamed Electroplating Questions 4 01-21-2007 10:07 AM
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 07:35 AM
Copy Chrome Start-up Elitefisherman Electroplating Questions 10 04-18-2004 04:24 AM
Copy Chrome Questions junodale Electroplating Questions 13 03-17-2004 11:15 AM


All times are GMT -4. The time now is 01:10 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.