Default Removing old plating

Must I remove old nickel plating before tank plating. Can I plate then polish nickel and plate the same piece again for higher luster? Also, for small parts (three inch by 1/4 inch strips of .040" steel) is brush plating better than tank plating? Thanks in advance.
Reply With Quote
  #2 (permalink)  
Old 01-26-2003, 01:30 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

You can nickel plate over existing nickel plate. You have to use an acid pickle called Nickle Activator. It's in the manual.

Brush plating is good when you can't get an item in a tank for whatever reason, like plating a car emblem while still on the car. Tank plating generally gives a more uniform plate.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Removing Tin Plating gsw3 Electroplating Questions 2 05-06-2005 09:16 PM
Removing copper plating.......Help! Coltsaa Electroplating Questions 8 11-03-2004 11:34 PM
Removing copper plating? Help...... Coltsaa Other Metal Finishing Questions 0 10-11-2004 08:58 PM
Removing old plating model_t Electroplating Questions 1 12-16-2002 10:02 PM
Removing Nickel Plating drdarvocet Electroplating Questions 5 10-25-2002 07:55 PM


All times are GMT -4. The time now is 07:54 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.