I would like to plate shakudo (4%-6% gold in copper) onto a copper subtrate for subsequent patination. Shakudo takes on a dark black/purple hue when properly patinated.
Can a standard copper plating system & solution be used with a shakudo anode, or will the copper selectively plate out leaving the gold ... or vice versa? If necessary, can a copper plating / gold plating solution be combined? What brightener should I use to keep the plating uniform, smooth and bright with minimal oxygen inclusion? |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Keep getting blisters in flash copper plating...HELP | gtabadboy | Electroplating Questions | 7 | 11-17-2005 08:19 PM |
| Improving Plating Performance | jimcarry | Electroplating Questions | 0 | 09-28-2005 08:50 AM |
| I did a dumb thing - now how do I remove copper plating? | Mark3316 | Other Metal Finishing Questions | 0 | 05-19-2005 02:57 PM |
| Differet copper plating questions, plus copy chrome/ nickel? | krsimulis | Electroplating Questions | 1 | 07-26-2004 12:25 AM |
| Silver Plating on Copper | hparent | Electroplating Questions | 1 | 04-03-2002 05:16 PM |