would it be alright to use water from a dehumidifier in my anodizing tank ?
I am not sure if the water would pick up oxidation from the copper coils.Any information would be helpful. |
|
||||
|
Use it as final rinse water, just in case. Don't use it in your solutions.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| trouble plating with 18K fast gold solution | didierphmartin | Electroplating Questions | 2 | 05-06-2008 02:51 PM |
| Copy Cad acidity question | aermakov@rogers.com | Electroplating Questions | 1 | 05-16-2004 10:32 AM |
| Peak voltage question | mudwhump | Anodizing Questions | 6 | 01-14-2004 10:53 PM |
| Odd shape question | carmelmike | Electroplating Questions | 2 | 03-17-2003 10:08 PM |
| 14k gold solution | Rusty Armstrong | Electroplating Questions | 1 | 04-05-2002 10:23 PM |