Old 01-14-2007, 06:10 PM
Newbie
 
Join Date: Jan 2007
Posts: 1
inacoma is on a distinguished road
Default hard chrome a gun

Hello,

I've done quite a bit of polishing and what not with your products, but no hard chroming. Hard chroming is very popular on firearms. I've read and heard it is very difficult to do:

http://www.trippresearch.com/chrome/chrome.htm

...this is "cobra chrome"...however I believe it's a proprietary form of hard chroming.

Does your kit successfully hard chrome hand guns?

thanks!

K
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
hard chrome plating dcarter Electroplating Questions 4 04-27-2008 10:21 PM
Hard Chrome Problem pppoffice Electroplating Questions 4 08-26-2005 04:42 AM
Hard Chrome Plating Help dg5240 Electroplating Questions 0 05-31-2005 03:17 PM
Nickel first before hard chrome? Daveleeander Electroplating Questions 0 12-02-2004 11:13 AM
Hard chrome vs triple chrome butters Electroplating Questions 1 02-19-2003 11:35 PM


All times are GMT -4. The time now is 01:52 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.