I looking to Zinc Plate some Stainless Bolts and Nuts. I would like to get the original Yellow Dichromate Finish, with the long term durability of Stainless. Has anybody tried this? I have about 80 Nuts and Bolts, and it does pay to take the original items to a plating service. Given there odd size and Yellow Dichromate Finish, new ones are too pricey. I though SS and plating would be a good combination, original look with long term durability of SS.
Your input would be helpful. |
|
||||
|
You'll need a nickel plating kit, with some Stainless Steel Activator crystals and a zinc plating kit with yellow chromate crystals.
You plate with Stainless Steel Activator first, then zinc plate, then dip in the Yellow Chromate. Should work very well.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Zinc plating on running seal surface? | Broke | Electroplating Questions | 1 | 12-06-2004 01:52 PM |
| CopyCad & Zinc failure - electrolyte problems? | seanc | Electroplating Questions | 4 | 11-08-2004 09:16 AM |
| NEED HELP QUICK!!! Yellow Zinc Plating Fasteners | BryanD | Electroplating Questions | 1 | 05-01-2004 12:34 PM |
| Copper plating on stainless steel 316L strip/sheet | slee36 | Services Offered/Wanted | 0 | 03-31-2004 12:46 PM |
| Plating Tank - Zinc | aermakov@rogers.com | Electroplating Questions | 1 | 03-27-2003 01:38 PM |