Our PNP copper is our Flash Copper Formula - alkaline, not acid.
We do make an acid copper available in 8oz bottles, but you'll need to call us. All of our plating solution's formulae are trade secret.
__________________
-- Lance Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm Please support the moderators on our site by leaving reputation for their helpful posts. Read more here. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Flash Copper Problem | gwjohnso | Plating Pot Metal | 12 | 02-27-2007 11:41 PM |
| PnP copper solution | kittykitty1979 | Electroplating Questions | 1 | 02-16-2007 11:34 AM |
| Strike Copper or Acid Copper over Nickel? | mdarr | Electroplating Questions | 2 | 07-13-2003 01:53 AM |
| Strike copper or bright copper after zincate? | mdarr | Electroplating Questions | 2 | 06-29-2003 02:23 PM |