From the EN Page:
Our 1/2 Gallon kit (1 Liter) will plate approx. 150 sq. in. of surface area with a bright nickel @ 1 mil, or 600 sq. in. @ 0.25 mil.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
||||
|
What exactly is this part? To electroless nickel plate, you need to be able to immerse the entire part in the supplied tank...sounds like this might be a little big for a 1/2 Gallon Kit.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
||||
|
Well, the 1/2 Gallon kit comes with a tank that is 7" diam x 6" deep. I doubt you'll get all eight in there.
If you send me an e-mail to webmaster@caswellplating.com, I'll send you the instruction booklet.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 10:11 AM |
| Nickel bath inexplicably quits plating | jackf | Electroplating Questions | 5 | 01-25-2005 10:55 PM |
| Brass Plating Tank | agugliel75 | Electroplating Questions | 7 | 02-06-2004 09:50 AM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 03:52 AM |
| Electroless Krome plating Q's | chcarver | Electroplating Questions | 1 | 10-10-2002 11:00 PM |