Default Gold over existing gold plate

I have a 15 year old Seiko GP watch with a somewhat faded case and bracelet. The base matal is stainless but there is still significant goldplate on the watch. Can I brush directly over it or do I need to remove it and nickel plate first.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
looking to plate gold over silver Daktion Electroplating Questions 0 04-26-2006 12:19 PM
Plug n Plate Gold over Sterling novenarosary Electroplating Questions 0 03-12-2004 11:00 PM
Stripping gold plate brg404 Electroplating Questions 0 10-08-2003 11:54 AM
Chrome Plug 'N Plate over gold finish ntd Electroplating Questions 2 06-18-2003 12:04 AM
Silver polish on 24k gold plate?? chromo Electroplating Questions 3 04-07-2003 06:14 AM


All times are GMT -4. The time now is 09:48 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.