Default Stripping Gun Blue & Black Oxide

What is the best way (chemical) to remove an existing gun blue, or black oxide finish on a soft carbon steel base, without altering the base itself?
Reply With Quote
  #2 (permalink)  
Old 03-02-2003, 10:18 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

http://www.caswellplating.com/bbs/viewtopic.php?t=643
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 03-03-2003, 12:12 AM
Newbie
 
Join Date: Mar 2003
Posts: 3
damnedin82
Default acid

Is muratic the same as muriatic (pool supply) acid? What concentration (ratio) should be used?
Reply With Quote
  #4 (permalink)  
Old 03-05-2003, 02:11 PM
Newbie
 
Join Date: Feb 2003
Posts: 9
jim_poter
Default gun blue removal

well i always use muratic pool acid strait it does a great job on removing blue then i rinse in distilled water prior to plateing
Reply With Quote
  #5 (permalink)  
Old 03-30-2006, 12:00 AM
Newbie
 
Join Date: May 2005
Posts: 2
gregwilkinson
Default Re: Stripping Gun Blue & Black Oxide

Quote:
Originally Posted by mcaswell
Hi Mike,
I tried clicking on this link which seems to be out of date. Do you have a current link for stripping black oxide?

Thank you,
Greg
Reply With Quote
  #6 (permalink)  
Old 03-30-2006, 02:37 PM
lcaswell's Avatar
Caswell Inc President
 
Join Date: Jan 2001
Location: Lyons NY USA
Posts: 2,361
Blog Entries: 3
lcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud of
Default Re: gun blue removal

Quote:
Originally Posted by jim_poter
well i always use muratic pool acid strait it does a great job on removing blue then i rinse in distilled water prior to plateing
What Jim said....muriatic acid.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote
  #7 (permalink)  
Old 03-31-2006, 12:07 AM
Newbie
 
Join Date: May 2005
Posts: 2
gregwilkinson
Default Re: Stripping Gun Blue & Black Oxide

Thank you Lance.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Need Help w/ Black Oxide Kit salezdroid Other Metal Finishing Questions 3 11-18-2004 07:54 AM
black oxide - impressive cray Other Metal Finishing Questions 0 11-03-2004 12:05 PM
Black Oxide vs. Parkerizing ar15dcm Other Metal Finishing Questions 1 07-02-2004 02:59 PM
How Good is Black Oxide bhysjulien Other Metal Finishing Questions 9 05-24-2004 10:12 PM
Bluing shotgun barrels with Black Oxide? Beach004 Electroplating Questions 1 10-04-2003 10:18 AM


All times are GMT -4. The time now is 03:29 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.