I HAVE MY TRIPLE CHROME PLATING TANKS SET UP, WOO HOO,
The book is a bit confusing to me though, lets see if I got this right, Lets say I want to chrome plate a bolt, first i clean it in degreaser, then water break test it, then put it in the flash copper tank, I dont need the acid copper because it dont need repair. then I polish the flash copper, water break it again then put it in the nickel,polish it again then into chrome, Is this correct |
|
|||
|
after each polish if needed, you have to re-clean, if you go from copper to nickel to chrome rinse in regular water after each step as well, never let a part dry either.
bill
__________________
http://home.comcast.net/~jhodges87/wsb/index.html |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| powder coat removal question | eliasson | Powder Coating Questions | 29 | 04-20-2007 08:28 AM |
| Newbie question about coverage | ublinkd | Powder Coating Questions | 4 | 03-05-2007 12:00 PM |
| Oven Glass Question | JTW37 | Oven Building Forum | 12 | 02-18-2007 01:01 AM |
| Peak voltage question | mudwhump | Anodizing Questions | 6 | 01-14-2004 10:53 PM |
| Brand Newbie Aluminum Polishing Question | gdsegel | Metal Polishing Questions | 1 | 04-25-2003 08:04 AM |