In the Caswell Plating manual Version 9 on page 29 it says to use 8 oz SP degreaser for 1 gallon of water: in the chart on page 36 it says 12 oz for three gallons of water.
Which solution is correct? Gardner |
|
|||
|
I just got the new tripple chrome kit and a the latest manual. My directions as stated on the packages of SP degreaser(2lb pack) states 1lb of crystals per 2 gal of distilled water, you will need 4 gal of water to mix with one pack of crystals.
Hope this helps Also, I have found out the hard way, you must get this stuff hotter than the fire pits of hell to get the best results. Sincerley Roger |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| trouble plating with 18K fast gold solution | didierphmartin | Electroplating Questions | 2 | 05-06-2008 02:51 PM |
| PNPG12 24ct gold brush plating solution | jerrylim | Electroplating Questions | 1 | 05-28-2007 02:42 AM |
| Black Chromate Solution - Particles in solution | MadChemist | Electroplating Questions | 0 | 01-25-2007 02:08 PM |
| Gold solution seperated.... | idahodewitt | Electroplating Questions | 0 | 01-21-2006 05:07 PM |
| SP Degreaser | aermakov@rogers.com | Electroplating Questions | 5 | 05-13-2003 09:55 PM |