I opened up my second jar of Copy Cad chrystals today and do have a question. I am no chemist, but the jar should contain just chloride(s) in powder form, why is there some brownish liquid? What is that? There is not much of it, but has me concerned a little. Please answer. Thanks. Andrew. |
|
||||
|
That's normal. We make it up as a super saturated liquid.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| triple chrome vs. nickel/chrome vs. copy chrome | spectraflamed | Electroplating Questions | 4 | 01-21-2007 11:07 AM |
| Copy Chrome? / Temp? | hefrod | Electroplating Questions | 4 | 08-18-2005 03:47 PM |
| Copy Chrome Start-up | Elitefisherman | Electroplating Questions | 10 | 04-18-2004 05:24 AM |
| Copy Chrome II on Pot Metal | wbrown | Plating Pot Metal | 1 | 04-09-2003 09:15 AM |
| Copy chrome as a strike plate | SUPRARACER | Electroplating Questions | 2 | 03-12-2003 03:36 PM |