I leave my acid copper and my flash copper anodes in because I plate with them about every day they set no longer than 3 days without use. how offen should I pull them and clean? Thanks Todd Breaden
|
|
|||
|
i took mine out simply because i didnt plate on a daily basis, if you plate each day i would not remove them.
bill
__________________
http://home.comcast.net/~jhodges87/wsb/index.html |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Flash Copper Problem | gwjohnso | Plating Pot Metal | 12 | 02-27-2007 11:41 PM |
| Strike Copper or Acid Copper over Nickel? | mdarr | Electroplating Questions | 2 | 07-13-2003 01:53 AM |
| Copper Anode Usage | mdarr | Electroplating Questions | 1 | 07-13-2003 12:11 AM |
| Strike copper or bright copper after zincate? | mdarr | Electroplating Questions | 2 | 06-29-2003 02:23 PM |