I have a large pile of nuts, bolts & washers I'd like to plate using my Copy-Cad kit. Would it be possible to plate them all in a bunch by putting them into a metal basket instead of hanging them individually or in a metal strip? I could agitate the basket occassionally to insure that all the surfaces get exposed to the electrolyte.
Just a thought.
__________________
Matt Harwood Harwood Performance Engineering Cleveland, OH Matt's 1941 Buick Century Restoration |
|
||||
|
Yes, but the basket will plate also and needs to be included in your surface area calculations.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Small Parts Plating in or around San Francisco, CA | ckm | Services Offered/Wanted | 0 | 05-17-2005 05:18 PM |
| Need Nickel Plating (small job) in NYC (could use mail) | higginsjr | Services Offered/Wanted | 0 | 03-10-2004 10:14 AM |
| Plating computer parts? Platis, metal, painted, buttons | chromo | Electroplating Questions | 0 | 09-05-2003 09:20 PM |
| Very very small parts and copper/nickel | xiphmont | Electroplating Questions | 2 | 10-23-2002 08:02 AM |
| Plating really small objects | edsel | Electroplating Questions | 1 | 06-13-2002 07:10 PM |